2115-1-thumbApplied Test Systems is the leader in reliable, long lasting, precise direct load test systems. When combined with our wide range of accessory equipment these machines are capable of performing many types and variations of creep and stress rupture testing.

Features

  • Compact frame with four, six, or eight independently controlled test stations
  • Standard Load capacity is 400 lbf. (1.7kN) per station
  • Optional accessories include:
  • High-temperature furnaces
  • Ovens / cooling chambers
  • Extensometers
  • Displacement transducers
  • Pneumatic weight elevators
  • Compression test fixtures
  • Calibrated load weights

Available with both manual controls and the WINCCS Computer control/ data acquisition system.